MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
General Plastics LAST-A-FOAM® FR-4618 Foam
Categories: Other Engineering Material

Material Notes: Product Description: The LAST-A-FOAM®FR-4600 Microcell Series supports the most intricate detail while eliminating extra prep work. With an even-smoother surface finish than our LAST-A-FOAM® FR-4500 material, they are superb for prototypes and models, and precision tooling applications. Advanced microcell technology creates a grain-free, ultra smooth exterior for painted finishes, significantly reducing process time. What’s more, its finer cell structure is comparable to higher-density foam products without the added cost and weight.

Key Performance Benefits:

  • Ultra smooth finish
  • Lighter, less abrasive than syntactic boards
  • Creates intricate, 3-D details
  • Dimensionally stable
  • Special formulation allows creation of shavings when material is machined
  • Reduced cutting tool abrasion
  • Large sheets up to 60” x 120”
Applications:
  • 3-D Signage
  • Design prototypes
  • Appearance or “sight” models
  • Architectural models
  • Topographical maps
  • Tooling and molds for low temperature curing prepregs (<200ºF)
  • Decorative moldings

Information provided by General Plastics Manufacturing Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.288 g/ccASTM D1622
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 36ASTM D2240
Tensile Strength 670 psiPerpendicular to Rise; ASTM D1623
Flexural Strength 958 psiRise Parallel to Beam Thick.; ASTM D790
 968 psiRise Parallel to Test Span; ASTM D790
Flexural Modulus 32544 psiRise Parallel to Test Span; ASTM D790
 32684 psiRise Parallel to Beam Thick.; ASTM D790
Compressive Strength 553 psi
@Temperature 71.1 °C
Parallel to Rise; ASTM D1621
 553 psi
@Temperature 71.1 °C
Perpendicular to Rise; ASTM D1621
 777 psi
@Temperature 23.9 °C
Perpendicular to Rise; ASTM D1621
 792 psi
@Temperature 23.9 °C
Parallel to Rise; ASTM D1621
Compressive Modulus 17541 psi
@Temperature 71.1 °C
Perpendicular to Rise; ASTM D1621
 18567 psi
@Temperature 71.1 °C
Parallel to Rise; ASTM D1621
 23894 psi
@Temperature 23.9 °C
Perpendicular to Rise; ASTM D1621
 25920 psi
@Temperature 23.9 °C
Parallel to Rise; ASTM D1621
Shear Modulus 2.463 ksiRise Parallel to Specimen Thickness; ASTM C273
Shear Strength 0.249 ksiRise Parallel to Specimen Thickness; ASTM C273
 
Thermal PropertiesOriginal ValueComments
CTE, linear 30.0 µin/in-°F
@Temperature -34.4 - 71.1 °C
GP Method
Thermal Conductivity 0.329 BTU-in/hr-ft²-°FASTM C518
Glass Transition Temp, Tg 225 °FASTM E1824
 
Descriptive Properties
Closed Cell Content97%ASTM D6226
Tumbling Friability (%)0.220 mins at 60 rpm, ASTM C421

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGENR031 / 186817

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.