MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Solvay Engineered Polymers SEQUEL® E2200 TPO  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Olefinic Elastomer (TPO); Polyolefin

Material Notes: Description: SEQUEL® E2200 thermoplastic olefinic elastomer (TPO) is designed for thermoformed exterior and interior applications that require low-temperature toughness and high rigidity. This product is fully colorable and is available in both UV-stabilized and non-UV-stabilized options. It is most functional when used as substrate layer for INDURE® E1500HG to provide a structure with excellent cold temperature impact properties as well as high stiffness.

Applications: Substrate layer for E1500HG high gloss cap layer or general purpose monolith material for sheet extrusion and thermoforming.

Information provided by Solvay Engineered Polymers.

LyondellBasell acquired Solvay Engineered Polymers in 2008. This grade is not part of the current LyondellBasell product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.950 g/ccASTM D792
Linear Mold Shrinkage 0.010 - 0.014 cm/cmASTM D955
Melt Flow 0.60 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 26.0 MPaASTM D638
Elongation at Break 210 %ASTM D638
Flexural Modulus 1.379 GPaI.B., TAN, 0.5 in/min; ASTM D790
Izod Impact, Notched 12.0 ft-lb/inNB; ASTM D256
 1.30 ft-lb/in
@Temperature -30.0 °C
PB; ASTM D256
Gardner Impact >= 320 in-lb
@Temperature -30.0 °C
ASTM D5420-96
 >= 320 in-lb
@Temperature 23.0 °C
ASTM D5420-96
 
Thermal PropertiesOriginal ValueComments
CTE, linear 81.2 µm/m-°C
@Temperature 20.0 °C
modified; ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 110 °CASTM D648
Flammability, UL94 HBall colors

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOLE26 / 68032

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.