MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BCC Products DP-11-90 Urethane Casting
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: DP-11-90 is an unfilled, low viscosity, quick setting two component urethane system. An easy to use 1 to 1 mix ratio (Part A/Part B), DP-11-90 offers the user a 3 minute working time with parts demoldable in as little as 30 minutes. When properly cured, DP-11-90 will exhibit high impact strength and yield thermoplastic-like parts. Some features include the following: mercury free, moderate heat resistance, no objectionable odor, excellent finishing properties, turns tan color upon cure, and thermoplastic appearance.

Information provided by BCC Products, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/ccASTM D792-66
Brookfield Viscosity 176 cPPart A; ASTM D2393
 300 cPMixed
 450 cPPart B
Linear Mold Shrinkage 0.0025 cm/cmASTM D2566
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 72 - 78ASTM D2240-68
Elongation at Break 11.2 %ASTM D638
Flexural Modulus 296200 psi
 
Thermal PropertiesOriginal ValueComments
Heat Distortion Temperature 145 °F24 Hours at 75°F
 
Processing PropertiesOriginal ValueComments
Cure Time 30.0 - 60.0 min
@Temperature 25.0 °C
demold time
Gel Time 3.0 min
@Temperature 24.0 °C
200g; ASTM 2471-71
 
Descriptive Properties
Mix Ratio1:1 by weight or volume

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BCC Products BC 8405 Urethane Casting
BCC Products BC 8165 Urethane Casting
BCC Products BC 8400 Urethane Casting
BCC Products BC 8870 Polyurethane Elastomer
BCC Products Proto-Kast BC 8163 Urethane Casting

PBCC057 / 107284

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.