MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
SCG Chemicals ICORENE® 1314 High performance hexene linear medium density polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Medium Density (MDPE); Linear Medium Density Polyethylene (LMDPE), Rotational Molded

Material Notes: ICORENE® 1314 is high performance hexene linear medium density polyethylene specifically developed for use in rotational molding. ICORENE® 1314 is designed for use in many different rotomolding applications. It has been designed for applications requiring good stiffness and toughness. It can be used for Food Contact applications. Related Finished Products: Large tanks, Fuel oil tanks, Septic tanks.

Features: Good impact strength. Good stiffness.

Information provided by SCG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.939 g/ccAnneal; ASTM D 1505
ESCR 100% Igepal® >= 1000 hour
@Temperature 50.0 °C
ASTM D1693
Melt Flow 3.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 62ASTM D2240
Tensile Strength at Break >= 1000 MPaASTM D638
Tensile Strength, Yield 20.0 MPaASTM D638
Flexural Modulus 800 MPaASTM D790
Charpy Impact, Notched 13.0 kJ/m²
@Temperature 23.0 °C
ISO 178
Dart Drop Total Energy >= 200 J/cm
@Temperature -20.0 °C
Test based on ISO 6603
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 67.0 °CASTM D648
 
Descriptive Properties
AppearanceColored powder
 Natural powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSCGC731 / 277988

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.