(Viewing data as-entered.
Click here
to return)
Haysite 24500 Vinyl Ester BMC, 20% Glass Reinforced
Categories:
Polymer
;
Thermoset
;
Filled/Reinforced Thermoset
;
Polyester, TS
;
Thermoset Polyester Glass Filled BMC
;
Vinyl Ester
Material Notes:
The 24500 series bulk molding compound offers good mechanical performance and excellent resistance to corrosive agents. This grade is formulated with a vinyl ester resin system and can be compression, transfer, or injection molded.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.77
g/cc
ASTM D572
Water Absorption
0.29 %
ASTM D570
Mechanical Properties
Original Value
Comments
Tensile Strength, Ultimate
48.0
MPa
Flexural Strength
159
MPa
Compressive Strength
145
MPa
Izod Impact, Notched
5.90
J/cm
edgewise; ASTM D256
Electrical Properties
Original Value
Comments
Dielectric Strength
15.0
kV/mm
Perpendicular (ASTM D149), Short Time
Arc Resistance
187
sec
ASTM D495
Thermal Properties
Original Value
Comments
Maximum Service Temperature, Air
130
°C
temperature rating
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
A. Schulman BMC 845 30% Glass Filled Vinyl Ester
A. Schulman BMC 845 Vinyl Ester Molding Compounds, 30% Glass-Filled
Quantum Composites QC-8805 66% Glass Fiber Vinyl Ester SMC
Quantum Composites QC-8100 60% Glass Fiber Vinyl Ester SMC
Haysite 44500 Vinyl Ester SMC, 30% Glass Reinforced
PHAY04 / 45610
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.