MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Haysite 48600 Polyester SMC, 30% Glass Reinforced
Categories: Polymer; Thermoset; Composite SMC; Filled/Reinforced Thermoset; Polyester, TS; Thermoset Polyester Glass SMC

Material Notes: The 48600 series sheet molding compound is formulated with a high temperature resin system (180º C). Designed for compression molding, this grade offers excellent retention of physical and electrical properties after exposure to elevated temperatures.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.58 g/ccASTM D572
Water Absorption 0.235 %ASTM D570
Linear Mold Shrinkage 0.0010 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 90.0 MPa
Flexural Strength 172 MPa
Compressive Strength 103 MPa
Izod Impact, Notched 10.7 J/cmedgewise; ASTM D256
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 17.0 kV/mmPerpendicular (ASTM D149), Short Time
Arc Resistance 100 secASTM D495
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 180 °Ctemperature rating

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Haysite 43000 Polyester SMC, 22% Glass Reinforced
Haysite 46000 Polyester SMC, 30% Glass Reinforced
Applied Composites 150 Polyester SMC
Applied Composites 179 Polyester SMC
Applied Composites 185 Polyester SMC

PHAY12 / 45618

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.