MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Total PS CPDS 853 Flame Retardant Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Flame Retardant

Material Notes: POLYSTYRENE (PS) COMPOUND (CPDS) 853 is a high impact, high stiffness halogen free flame retardant polystyrene.

Main Characteristics:

  • Bromine and Chlorine free,
  • UL94 V2 @ 1.6 mm with very low combustion time,
  • Good flow and UV properties.

Applications: Covers for electrical equipment, TV covers, office automation.

Information provided by Total Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.06 g/ccISO 1183
Water Absorption <= 0.10 %ISO 62
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
Melt Flow 5.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ISO 1133H
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 32.0 MPaISO 527-2
Elongation at Break 40 %ISO 527-2
Flexural Modulus 2500 MPaISO 178
Izod Impact, Notched (ISO) 7.00 kJ/m²180/1A
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 81.0 °C
@Load 5.10 kg
50°C per hour; ISO 306B50
Flammability, UL94 V-2
@Thickness 1.60 mm
All colors
 
Processing PropertiesOriginal ValueComments
Melt Temperature <= 300 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Total PS CPDS 818E Flame Retardant Polystyrene
LG Chemical HIPS 460AF PS, Flame Retardant
Ineos Nova Zyntar® 779 High Performance Flame Retardant Polystyrene

PTOTAL899 / 130624

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.