MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Universal Wire Works 410 Stainless Steel Electrode
Categories: Metal; Ferrous Metal; Stainless Steel; T 400 Series Stainless Steel

Material Notes: Universal 410 is a 12% straight chromium electrode used for the welding of type 410 stainless steel in the fabrication of equipment that demands corrosion resistance, good strength and ductility. Alloy 410 is an air hardening material and therefore requires preheat and postweld heat treatments to achieve adequate ductility in the weld deposits. Alloy 410 electrodes provide good corrosion and oxidation resistance at temperatures up to 1500 degrees F. Deposits are martens tic and therefore not subject to carbide precipitation. Alloy 410 may also be used for welding types 403, 405, 414, 416, and 420 stainless steels and overlaying carbon steels to provide resistance to corrosion, erosion and abrasion.

Information provided by Universal Wire Works for their line of welding wire and filler metal.

Key Words: AWS E410-15,16
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 82000 psi
Elongation at Break 31 %
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 1500 °F
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.11 %
Chromium, Cr 12.2 %
Iron, Fe 86.5 %As Remainder
Manganese, Mn 0.75 %
Silicon, Si 0.45 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
MetalTek MTEK 440C Cast UNS J91639 Martensitic Stainless Steel
MetalTek MTEK H46 Martensitic Stainless Steel
Sandvik Osprey 420 Stainless Steel Powder (Grade 80% - 22)
Sandvik Osprey 420/MA Stainless Steel Powder (Grade 80% - 22)
FloMet 430L Stainless Steel

NUWW028 / 19600

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.