MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Trinseo CALIBRE™ 5201 15 Polycarbonate, 20% Glass Reinforced  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, 20% Glass Filled

Material Notes: CALIBRE® 5201 is a 20% glass reinforced polycarbonate resin containing mold release for optimal processing. CALIBRE 5201 resin exhibits high modulus and excellent dimensional stability.

CALIBRE 5201 polycarbonate resin is typically used for electrical boxes, lighting components and electrical connectors.

Available Melt Flow Rate: 15.

Data provided by Dow Chemical.

This product line was spun off from Dow Chemical to Styron in 2010.

Key Words: PC
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.33 g/ccASTM Data
Melt Flow 15 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM Data
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 82.7 MPaASTM Data
Tensile Strength, Yield 60.0 MPaISO Data
Elongation at Break 4.0 %ASTM Data
Elongation at Yield 2.0 %ISO Data
Tensile Modulus 5.17 GPaASTM Data
Izod Impact, Notched 1.07 J/cmASTM Data
Charpy Impact Unnotched 7.00 J/cm²ISO Data, Low Temp
 NBISO Data
Charpy Impact, Notched 1.00 J/cm²ISO Data, Low Temp
 1.20 J/cm²ISO Data
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 138 °CUnannealed; ASTM Data
Vicat Softening Point 154 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Trinseo CALIBRE™ 5201-12 Polycarbonate Resin
Trinseo CALIBRE™ 5201-8 Polycarbonate Resin
Celanese Celanex® 5201 15% Fiberglass Reinforced Polyester
Trinseo EMERGE™ 8600-10 Polycarbonate
Aclo Accucomp Polycarbonate POL052L High Viscosity

PZZDW029 / 34260

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.