MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
SABIC LEXAN™ OQ3820 PC (Asia)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: High Viscosity, UV-stabilized grade for ophthalmic lenses.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.19 g/ccASTM D792
Density 1.20 g/ccISO 1183
Water Absorption 0.32 %23°C/sat; ISO 62
Moisture Absorption 0.150 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0060 - 0.0080 cm/cm
@Thickness 3.20 mm
SABIC method
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 6.0 g/10 min
@Load 1.20 kg,
Temperature 300 °C
cm³/10 min; ISO 1133
 7.4 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 71.0 MPa50 mm/min; ISO 527
 72.0 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 61.0 MPa50 mm/min; ISO 527
 62.0 MPa50 mm/min; ASTM D638
Elongation at Break 125 %50 mm/min; ASTM D638
 140 %50 mm/min; ISO 527
Elongation at Yield 6.0 %50 mm/min; ISO 527
 6.3 %50 mm/min; ASTM D638
Tensile Modulus 2270 MPa50 mm/min; ASTM D638
 2400 MPa1mm/min; ISO 527
Flexural Yield Strength 93.0 MPa1.3 mm/min, 50 mm span; ASTM D790
 94.0 MPa2 mm/min; ISO 178
Flexural Modulus 2200 MPa2 mm/min; ISO 178
 2410 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 918 J/mASTM D256
 14.0 J/m
@Temperature -30.0 °C
ASTM D256
Izod Impact, Notched (ISO) 70.0 kJ/m²80*10*3; ISO 180/1A
 12.0 kJ/m²
@Temperature -30.0 °C
80*10*3; ISO 180/1A
Izod Impact, Unnotched (ISO) NB80*10*3; ISO 180/1U
 NB
@Temperature -30.0 °C
80*10*3; ISO 180/1U
Charpy Impact Unnotched NBEdgew 80*10*3 sp=62mm; ISO 179/1eU
 NB
@Temperature -30.0 °C
Edgew 80*10*3 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 75.0 kJ/m²Edgew 80*10*3 sp=62mm; ISO 179/1eA
 15.0 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*3 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 85.0 JASTM D3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 76.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
 77.4 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
CTE, linear, Transverse to Flow 77.4 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 78.9 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Hot Ball Pressure Test 75.0 °CIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 139 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 126 °C1.8 MPa Edgew 120*10*4 sp=100mm; ISO 75/Ae
 129 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 143 °CRate B/50; ISO 306
 144 °CRate B/120; ISO 306
 150 °CRate B/50; ASTM D1525
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 305 - 325 °CInjection Molding
Zone 1 290 - 310 °C
Zone 2 300 - 320 °C
Zone 3 310 - 330 °C
Melt Temperature 310 - 330 °C
Mold Temperature 80.0 - 115 °C
Drying Temperature 120 °CInjection Molding
Dry Time 3.00 - 4.00 hourInjection Molding
 48.0 hourCumulative; Injection Molding
Moisture Content 0.020 %
Back Pressure 0.300 - 0.700 MPa
Shot Size 40 - 60 %
Vent Depth 0.00250 - 0.00760 cm
Screw Speed 40 - 70 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10526 / 243993

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.