PREBLACK PS 720-35 is a black PS-based masterbatch developed for the coloring of extruded and injection molded products made of polystyrenes and ABS. Due to the good carbon black dispersion and hiding power of PREBLACK PS 720-35 it is well suited for demanding applications at low dosage levels. Information provided by Premix Thermoplastics Inc. |