MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
ITW Plexus® MA3940LH Methacrylate Adhesive
Categories: Polymer; Adhesive; Thermoset; Methacrylate; Methacrylate Adhesive

Material Notes: Plexus® MA3940LH is a new generation of fast-setting two-part methacrylate adhesives specifically designed for the structural assembly of advanced automotive components1. Combined at a 10:1 ratio, it has a working time of 4 to 5 minutes and achieves 75% of ultimate strength in 8 to 10 minutes. After mixing, Plexus MA3940LH cures rapidly to form a tough, elastomeric bond with superb shear, peel, fatigue, and impact strength over a wide temperature range. In addition, this product has superior toughness at temperatures below -17°C. Plexus MA3940LH is off white and is supplied in ready-to-use cartridge, 5-gallon (20-liter) pails, or 50-gallon (200-liter) drums to be dispensed as a non-sagging gel.

Excellent resistance to:  Acids and Bases (pH 3-10), Salt Solutions.  Susceptible to: Polar Solvents, Strong Acids and Bases.  Adhesive color;  off white (uncured-room temperature).  Activator color:  off white (uncured-room temperature)

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.80 lb/galadhesive. Uncured.
 8.18 lb/galCured
 8.65 lb/galActivator. Uncured.
Volatile Organic Compounds (VOC) Content <= 10 g/lDuring cure
Viscosity 30000 - 70000 cP
@Temperature 22.2 °C
Activator
 120000 - 160000 cP
@Temperature 22.2 °C
Adhesive
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 1160 - 1740 psiASTM D638
Elongation at Break 75 - 100 %ASTM D638
Tensile Modulus 17700 - 20300 psiASTM D638
Adhesive Bond Strength 1200 - 1600 psiLap Shear Cohesive Strength; ASTM D1002
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 250 °F
Minimum Service Temperature, Air -40.0 °F
Flash Point 51.0 °F
 
Processing PropertiesOriginal ValueComments
Working Life 4.00 - 5.00 min
@Temperature 23.3 °C
Shelf Life 7.00 MonthCartridges
 7.00 MonthActivator (B side)
 13.0 MonthAdhesive (A side)
 
Descriptive Properties
Fixture Time (mins)8 to 10Room temperature cure. Fixture time varies with bond gap and ambient temperature. Present values were measured at 74°F.
Gap Filling (in)0.04 to 0.16Room temperature cure.
Mix Ratio by volume10 to 1Adhesive to Activator. Room temperature
Mix Ratio by weight8.9 to 1Adhesive to Activator. Room temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PITWP9016 / 239526

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.