MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Pressure Seal 8640 Fluorinated Hydrocarbon
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Compound 8640 is a 60 durometer black colored general purpose fluorinated hydrocarbon elastomer. It exhibits good resistance to heat, compression set and petroleum based oils. This compound will meet or exceed the specifications listed and has the following physical properties: ASTM D2000 2 HK 610 A1-10 B31 B38 EO78 F15; 4 HK 610 A1-11 B38 EO78; 6 HK 610 A1-10 A1-11 B31 B38 EO88 F15

Information provided by Pressure Seals Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.88 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 65
 55
@Temperature 200 °C,
Time 252000 sec
Stauffer Blend 7700
 60
@Temperature 200 °C,
Time 252000 sec
Service Fluid 101
 64
@Temperature 23.0 °C,
Time 252000 sec
ASTM Reference Fuel A
 64
@Temperature 23.0 °C,
Time 252000 sec
ASTM Reference Fuel C
 64
@Temperature 150 °C,
Time 252000 sec
ASTM Oil #1
 64
@Temperature 150 °C,
Time 252000 sec
ASTM Oil #3
 68
@Temperature 275 °C,
Time 252000 sec
Heat Aged
 68
@Temperature 100 °C,
Time 252000 sec
Distilled water aged
 70
@Temperature 250 °C,
Time 252000 sec
Heat Aged
Tensile Strength 1457 psi
 996.6 psi
@Temperature 23.0 °C,
Time 252000 sec
ASTM Reference Fuel C
 1117.5 psi
@Temperature 200 °C,
Time 252000 sec
Stauffer Blend 7700
 1146.7 psi
@Temperature 275 °C,
Time 252000 sec
Heat Aged
 1222.4 psi
@Temperature 200 °C,
Time 252000 sec
Service Fluid 101
 1471.57 psi
@Temperature 23.0 °C,
Time 252000 sec
ASTM Reference Fuel A
 1496.8 psi
@Temperature 150 °C,
Time 252000 sec
ASTM Oil #1
 1566.3 psi
@Temperature 150 °C,
Time 252000 sec
ASTM Oil #3
 1623.1 psi
@Temperature 250 °C,
Time 252000 sec
Heat Aged
Elongation, Ultimate 240 %
 10.08 %
@Temperature 250 °C,
Time 252000 sec
Heat Aged
 19.92 %
@Temperature 23.0 °C,
Time 252000 sec
ASTM Reference Fuel A
 49.92 %
@Temperature 275 °C,
Time 252000 sec
Heat Aged
 210 %
@Temperature 23.0 °C,
Time 252000 sec
ASTM Reference Fuel C
 240 %
@Temperature 150 °C,
Time 252000 sec
ASTM Oil #1
 240 %
@Temperature 200 °C,
Time 252000 sec
Stauffer Blend 7700
 270 %
@Temperature 150 °C,
Time 252000 sec
ASTM Oil #3
 280.08 %
@Temperature 200 °C,
Time 252000 sec
Service Fluid 101
100% Modulus 400 psi
Tear Strength 116 pliDie B
Compression Set 7.8 %
@Temperature 200 °C,
Time 79200 sec
Plied
 8.1 %
@Temperature 175 °C,
Time 79200 sec
Plied
 12.5 %
@Temperature 23.0 °C,
Time 79200 sec
Plied
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -15.0 °F
Shrinkage 0.00 %
@Temperature 23.0 °C,
Time 252000 sec
Volume, ASTM Reference Fuel A
 0.20 %
@Temperature 150 °C,
Time 252000 sec
Volume, ASTM Oil #1
 1.7 %
@Temperature 150 °C,
Time 252000 sec
Volume, ASTM Oil #3
 3.5 %
@Temperature 100 °C,
Time 252000 sec
Volume, Distilled water aged
 4.5 %
@Temperature 23.0 °C,
Time 252000 sec
Volume, ASTM Reference Fuel C
 11.4 %
@Temperature 200 °C,
Time 252000 sec
Volume, Service Fluid 100
 17.4 %
@Temperature 200 °C,
Time 252000 sec
Volume, Stauffer Blend 7700
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPRESL097 / 318307

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.