MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Daikin DAI-EL® G-551 Fluoroelastomer Terpolymer, 69% Fluorine Content
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: DAI-EL® G-551 is a cure-incorporated terpolymer designed for transfer and compression molding. It offers a balance of fluid resistance and low temperature flexibility.

Typical Applications: Gaskets, oil seals, diaphragms

Rheological Properties:
Temperature: 190°C
Frequency: 100 cpm
Strain: 0.5°
Test time: 6 min

Information provided by Daikin.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.84 g/cc
Mooney Viscosity 48
@Temperature 121 °C
ML 1+10
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 80
Tensile Strength at Break 15.3 MPa
Elongation at Break 220 %
100% Modulus 6.60 MPa
@Strain 100 %
Compression Set 21 %
@Temperature 175 °C,
Time 252000 sec
#214 O-ring; ASTM D395 Method B
 28 %
@Temperature 200 °C,
Time 252000 sec
#214 O-ring; ASTM D395 Method B
 
Thermal PropertiesOriginal ValueComments
Minimum Service Temperature, Air -14.0 °CLow Temperature Retraction, TR10
 -12.0 °CGehman Torsion T10; ASTM 1053-92A
 -8.00 °CLow Temperature Retraction, TR70
 -7.00 °CGehman Torsion T2; ASTM 1053-92A
Brittleness Temperature -21.0 °CEmbrittlement
 
Processing PropertiesOriginal ValueComments
Cure Time 0.700 mints2, scorch time
 0.900 mint'50, time to 50% cure
 1.30 mint'90, time to 90% cure
 10.0 min
@Temperature 190 °C
Press Cure
 24.0 hour
@Temperature 232 °C
Post cure
 
Component Elements PropertiesOriginal ValueComments
Fluorine, F 69 %
 
Descriptive Properties
ColorWhite to light yellow mass
MH23.3 dNmmaximum torque
ML1.8 dNmminimum torque
Test Formula100 phrDAI-EL® G-551
 3 phrMagnesium oxide
 30 phrMT Carbon Black (N-990)
 6 phrCalcium hydroxide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Schott CONTURAX® Pro Borosilicate Glass
Schott CONTURAX® Borosilicate Glass
Röchling Glastic BMC 1412 GTP Glass-Reinforced Polyester
Daikin DAI-EL® G-701 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content
Daikin DAI-EL® G-551 Fluoroelastomer Terpolymer, Bisphenol Curable Grade, 68.5% Fluorine Content

PDAIJ9846 / 209917

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.