The FH35 resin is a high-density polyethylene, copolymer of butene-1, produced by the solution process for flat die film extrusion with good mechanical properties. It contains antioxidant additives. Its applications include diapers, sanitary napkins, and other specialties. The FH35 resin is indicated to be in cast die film extruders under processing conditions comparable to the other linear medium density polyethylene of similar fluidity and density. |