Special features:- excellent dishwasher detergent resistance
- low thermoplasticity
- good adhesion
- without addition of organotin-containing compounds
Application:- non-stick coatings in combination with PTFE
- decorative coatings of cookware, household appliances and electric and gas heaters with a permanent thermal stability of 220 °C
Information provided by Evonik
|