MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Indium Corp. Indalloy® 84002 Flux #2 Specialty, Acid Based Liquid Flux
Categories: Fluid

Material Notes: Indalloy Flux #2 is a specialty acid based liquid flux formulated for the purpose of soldering high chromium containing alloys including stainless steel. Indalloy Flux #2 also has proven to be an effective flux for soldering to NiTi (Nitinol) alloys. Other metals for use with Indalloy Flux #2 are: copper, brass, lead, chrome, galvanized iron and steel.

Chloride Content: No Zinc or Other Heavy Metal Chlorides
Due to its corrosive nature, Indalloy Flux #2 is not recommended for electronics applications.

Cleaning: Warm water (< 50°C) and mechanical scrubbing

Solder Alloy Compatibility: Indalloy Flux #2 is compatible with all types of solders.

Information Provided by Indium Corporation

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.53 g/cc
pH 1.0 - 1.5
 
Thermal PropertiesOriginal ValueComments
Active Range 100 - 371 °C
 
Descriptive Properties
Flash PointNon-Flammable

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Indium Corp. 16-1081T Flux Thinner
Sandvik 25.10.4.L T1 Flux Cored Wire Electrodes
Wacker Silfoam® SP 150 Silicone Antifoam Emulsion
Superior Flux Superior No. 18 Brazing Powder Flux
Superior Flux Superior Acid Core Flux

NNIN906 / 131545

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.