MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
SCG Chemicals H555JA High density polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: SCG HDPE H555JA is a high density polyethylene resin with good environment stress cracking resistance and good organoleptic property. It is particularly designed for injection molding and continuous compression molding of caps and closures for the packaging beverages caps and closures. Related Finished Products: Caps and closures for carbonated soft drinks, hot fill beverages and water.

Applications: Beverage caps and closures (carbonated soft drink, sparkling water, still and mineral water, juice and tea).

Features: Good environmental stress cracking resistance. Good mechanical property. Good organoleptic property.

Information provided by SCG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.953 g/ccASTM D 1505
ESCR 10% Igepal® 20 hourF50, condition B, compression molded; ASTM D1693
Linear Mold Shrinkage, Flow 0.0252 in/in
@Thickness 2.00 mm
TPE Method
Linear Mold Shrinkage, Transverse 0.0233 in/in
@Thickness 2.00 mm
TPE Method
Melt Flow 1.8 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 64ASTM D2240
Tensile Strength at Break 34.3 MPacrosshead speed 50 mm/min; ASTM D638
Tensile Strength, Yield 25.5 MPacrosshead speed 50 mm/min; ASTM D638
Elongation at Break 1200 %crosshead speed 50 mm/min; ASTM D638
Flexural Modulus 1090 MPaASTM D790
Izod Impact, Notched 78.0 J/m
@Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Melting Point 131 °CASTM D2117
Deflection Temperature at 0.46 MPa (66 psi) 78.0 °CASTM D648
 
Descriptive Properties
AppearanceBlock pellet

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSCGC715 / 277972

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.