MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Covestro Bayhydrol® U XP 2757 Polyurethane Coating
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings; Thermoset; Polyurethane, TS

Material Notes: Bayhydrol U XP 2757 is an aliphatic, hydroxyl-functional polycarbonate ester-polyurethane dispersion, cosolvent-free. It is suitable as a binder for water-reducible two component polyurethane coatings, especially soft-touch and comfort coatings.

Properties / Applications: Bayhydrol U 2757 can be used in combination with flexible polyurethane dispersions, e.g. Bayhydrol UH 340/1, UH 650, UH 2305 and UH XP 2660 to formulate soft-touch coatings. In combination with polyacrylates, e.g. Bayhydrol A 2058 highly chemical resistant comfort coatings can be formulated. Suitable polyisocyanate components are e.g. Bayhydur® 302, 304, XP 2655 and also Desmodur® N 3600 and N 3900. Bayhydrol U 2757 is cosolvent-free. It can be used in the formulation of highly haptic soft-feel coatings. The product has high elasticity, good chemical resistance and good scratch resistance. As with any product, use of Bayhydrol U XP 2757 in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.07 g/cc
Volatiles 46 - 50 %1g/1h/125°C
pH 7.2 - 8.21:4 in demineralized water
Viscosity 300 - 1500 cPD= approx. 40 s-1
 
Chemical PropertiesOriginal ValueComments
Acid Value 9.0[mg KOH/g]
 
Descriptive Properties
Content1%OH
Minimum Film Forming Temperature<0°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCOVEST0169 / 201952

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.