MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik EUROPLEX® Film HC 0F045 PMMA  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Acrylic (PMMA)

Material Notes: Product: EUROPLEX® Film HC 0F045 is a weather resistant, transparent and optical quality co-extruded PMMA and PVDF film for graphic lamination systems. This film displays excellent performance in long term outdoor weathering without experiencing color change or yellowing. EUROPLEX® Film HC 0F045 provides high protection for other polymeric substrates against degradation caused by UV radiation. Due to its PVDF top layer, the film displays very good chemical resistance, anti-soiling and easy to clean effect.

Application: EUROPLEX® Film HC 0F045 can be laminated as a protective top layer onto polymeric films and sheets based on PVC, ABS, PC and ASA. Decorative films protected with EUROPLEX® on top can be thermoformed and laminated on different substrates, such as PVC profiles, or used in molding processes such as In-Molding Decoration. In labels or Graphic Arts, EUROPLEX® Film HC 0F045 can be used as a high quality clear overlay in laminate systems for high UV and weathering protection. Chemical resistant, anti-soiling and easy to clean effects are achieved.

Information Provided by Evonik CYRO. The former Evonik Methacrylates business has been sold to Röhm GmbH, although this trade name was disontinued prior to the sale.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.19 g/ccDIN 53479
Surface Tension 23 dynes/cmDIN 53364
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 38.0 MPaISO 527-3
Elongation at Break >= 50 %ISO 527-3
Elongation at Yield 6.0 %ISO 527-3
 
Optical PropertiesOriginal ValueComments
Haze 3.0 %ASTM D1003
Transmission, Visible >= 92 %ISO 13458-2
UV Transmittance <= 1.5 %
@Wavelength 280 - 380 nm
DIN EN 410

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical TR-558NS Transparent ABS, Antistatic, Natural and Colored Pellets
PTS Trilac® TR558-CL ABS- Transparent ABS
Corning Vycor® 7907 UV-Blocking Glass
Chi Mei Polylac® PA-758 ABS - Transparent
Aclo Accucomp ABS ABS881L Clear Grade

PEVONIL035 / 196239

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.