MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Ensinger Tecast Vekton™ 6PALM Premium Bearing Grade cast nylon (PA6)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: Tecast 6PALM contains both solid and liquid lubricants dispersed throughout the nylon to provide consistent wear rates and coefficients of friction.

Information Provided by Ensinger Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 110ASTM D785
Tensile Strength, Ultimate 8500 psiASTM D638
Elongation at Break 40 %ASTM D638
Flexural Strength 12800 psiASTM D790
Flexural Modulus 400000 psiASTM D790
Izod Impact, Notched 1.75 ft-lb/inASTM D256
Coefficient of Friction, Dynamic 0.14
Coefficient of Friction, Static 0.16ASTM D3702
K (wear) Factor 49.0 x 10-10 in³-min/ft-lb-hrASTM D3702
Limiting Pressure Velocity 16000 - 17000 psi-ft/min
 
Thermal PropertiesOriginal ValueComments
CTE, linear 40.0 - 50.0 µin/in-°F
@Temperature 20.0 °C
ASTM D696
Maximum Service Temperature, Air 200 °FContinuous
 330 °FIntermittent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials Delrin® 100 AF Acetal Extruded Teflon® Filled Acetal
Akro-Plastic Akromid® B3 1 L natural (4685) PA6 + PP, Dry, 30% Glass Filled
Akro-Plastic Akromid® B3 GF 40 1 L black (4581) PA6 + PP Conditioned, 40% Glass Filled, Heat Stabilized
RTP Company RTP PA6 30 GF BLK Nylon 6 (PA), Value Product - Glass Fiber - Heat Stabilized
Ensinger ENSILON® 6/6 Extruded Nylon 6/6 (PA66)

PENS66 / 35993

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.