MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Westlake Epolene® C-23 LDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: Epolene C-23 is a branched low density polyethylene with a relatively high melt point and viscosity compared to other Epolene C-type Polymers. It is useful to modify paraffin wax to improve grease resistance, blocking temperature, scuff resistance, and gloss. Epolene C-23 is commonly used for extrusion coating of board stock. Epolene C-23 has good high temperature stability, low color and low temperature flexibility. Key Attributes: Enhances paraffin wax coating properties like gloss, grease resistance, and MVTR, Excellent thermal stability, Low color, Medium molecular weight. Application/Uses: Extrusion coating, Wax Modification.

Information provided by Westlake Chemical Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.910 g/ccASTM D4883
Melt Index of Compound 80 g/10 minASTM D1238

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Westlake Epolene® C-13P Coating Grade - Branched Medium Molecular Weight Polyethylene Polymer
Versalis Riblene® MV 10 R Low Density Polyethylene - Injection Molding
Celanese 192 LDPE polymer for adhesives, automotive and compounds
Celanese 191A LDPE polymer for adhesives, automotive and compounds
Borealis Borstar® FB2230 LLDPE for Film

PWESF8805 / 222877

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.