MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Film Grade
Categories: Polymer; Film; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Film Grade

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Film Grade". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.921 - 0.970 g/ccAverage value: 0.934 g/cc Grade Count:251
Water Absorption 0.100 %Average value: 0.100 % Grade Count:3
Moisture Vapor Transmission 0.590 - 0.940 cc-mm/m²-24hr-atmAverage value: 0.789 cc-mm/m²-24hr-atm Grade Count:8
Water Vapor Transmission 85.3 g/m²/dayAverage value: 85.3 g/m²/day Grade Count:3
Oxygen Transmission 158 - 229 cc-mm/m²-24hr-atmAverage value: 199 cc-mm/m²-24hr-atm Grade Count:8
Oxygen Transmission Rate 8900 cc/m²/dayAverage value: 8900 cc/m²/day Grade Count:3
Viscosity 2.00e+6 - 2.00e+6 cP
@Temperature 190 - 190 °C
Average value: 2.00e+6 cP Grade Count:2
 2.00e+6 - 2.00e+6 cP
@Shear Rate 50.0 - 50.0 1/s
Average value: 2.00e+6 cP Grade Count:2
Environmental Stress Crack Resistance 500 hourAverage value: 500 hour Grade Count:16
Vinyl Acetate Content 2.00 - 29.5 %Average value: 12.0 % Grade Count:129
Thickness 15.0 - 300 micronsAverage value: 53.3 microns Grade Count:118
Melt Flow 0.190 - 135 g/10 minAverage value: 3.07 g/10 min Grade Count:254
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 62.0 - 96.0Average value: 84.7 Grade Count:54
Hardness, Shore D 23.0 - 94.0Average value: 40.8 Grade Count:70
Tensile Strength, Ultimate 3.40 - 33.0 MPaAverage value: 15.6 MPa Grade Count:60
Film Tensile Strength at Yield, MD 3.00 - 15.0 MPaAverage value: 7.17 MPa Grade Count:96
Film Tensile Strength at Yield, TD 2.00 - 11.0 MPaAverage value: 6.49 MPa Grade Count:96
Tensile Strength, Yield 3.40 - 10.0 MPaAverage value: 8.00 MPa Grade Count:45
Film Elongation at Break, MD 100 - 1000 %Average value: 381 % Grade Count:192
Film Elongation at Break, TD 260 - 1000 %Average value: 617 % Grade Count:192
Film Elongation at Yield, MD 6.40 - 19.4 %Average value: 9.03 % Grade Count:25
Film Elongation at Yield, TD 5.40 - 16.0 %Average value: 7.44 % Grade Count:25
Elongation at Break 50.0 - 1200 %Average value: 579 % Grade Count:77
Modulus of Elasticity 0.00500 - 0.338 GPaAverage value: 0.159 GPa Grade Count:54
Flexural Modulus 0.0190 - 0.145 GPaAverage value: 0.0708 GPa Grade Count:25
Secant Modulus 0.00500 - 1.05 GPaAverage value: 0.143 GPa Grade Count:22
Secant Modulus, MD 0.0241 - 0.600 GPaAverage value: 0.117 GPa Grade Count:146
Secant Modulus, TD 0.0248 - 0.700 GPaAverage value: 0.135 GPa Grade Count:146
Tensile Impact Strength 146 - 815 kJ/m²Average value: 596 kJ/m² Grade Count:16
Coefficient of Friction 0.100 - 3.40Average value: 0.536 Grade Count:32
Peel Strength 0.00105 - 6.00 kN/mAverage value: 1.00 kN/m Grade Count:4
Elmendorf Tear Strength MD 40.0 - 600 gAverage value: 198 g Grade Count:75
Elmendorf Tear Strength TD 30.0 - 345 gAverage value: 129 g Grade Count:70
Elmendorf Tear Strength, MD 0.197 - 18.9 g/micronAverage value: 4.89 g/micron Grade Count:88
Elmendorf Tear Strength, TD 0.945 - 9.06 g/micronAverage value: 3.75 g/micron Grade Count:76
Dart Drop 1.97 - 30.0 g/micronAverage value: 6.91 g/micron Grade Count:117
Dart Drop Test 70.0 - 1100 gAverage value: 309 g Grade Count:127
Film Tensile Strength at Break, MD 6.00 - 41.0 MPaAverage value: 26.7 MPa Grade Count:196
Film Tensile Strength at Break, TD 6.00 - 40.0 MPaAverage value: 24.1 MPa Grade Count:189
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+14 - 1.00e+15 ohm-cmAverage value: 3.25e+14 ohm-cm Grade Count:4
 
Thermal PropertiesOriginal ValueComments
Melting Point 63.9 - 110 °CAverage value: 94.1 °C Grade Count:181
Crystallization Temperature 85.0 - 96.0 °CAverage value: 90.9 °C Grade Count:16
Vicat Softening Point 44.0 - 96.0 °CAverage value: 75.8 °C Grade Count:177
Brittleness Temperature -90.0 - -76.0 °CAverage value: -79.6 °C Grade Count:27
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.48 - 1.49Average value: 1.48 Grade Count:12
Haze 0.900 - 28.0 %Average value: 5.98 % Grade Count:186
Gloss 17.0 - 123 %Average value: 73.1 % Grade Count:177
Yellow Index 2.90 - 8.20 %Average value: 5.71 % Grade Count:3
Transmission, Visible 10.0 - 92.0 %Average value: 86.3 % Grade Count:65
Reflection Coefficient, Visible (0-1) 0.0600 - 0.0900Average value: 0.0800 Grade Count:4
 
Processing PropertiesOriginal ValueComments
Processing Temperature 100 - 210 °CAverage value: 155 °C Grade Count:27
Melt Temperature 150 - 221 °CAverage value: 194 °C Grade Count:55
Die Opening 0.0635 - 0.150 cmAverage value: 0.0820 cm Grade Count:10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Molded/Extruded
Overview of materials for PVC, Flexible Grade
Arkema Evatane® 1003 VL 2 Ethylene Vinyl Acetate

O4107 / 78294

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.