MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Radici Heraflex ® E 7722 1000 NAT Thermoplastic Polyester Elastomer
Categories: Polymer; Thermoplastic; Polyester, TP; Polyester Thermoplastic Elastomer

Material Notes: TPC-ET Thermoplastic Elastomer. High modulus, nominal shore D/15s 69. Natural color.

Information provided by Radici Group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.25 g/ccISO 1183
Water Absorption 0.10 %
@Thickness 1.00 mm
Immersion; ISO 62
Melt Flow 19 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 77Instantaneous; ISO 7619-1
 69
@Time 15.0 sec
ISO 7619-1
Tensile Strength at Break 29.0 MPa5mm / min.; ISO 527-2/1A
Tensile Strength, Yield 48.0 MPa50mm/min.; ISO 527-2/1A
 32.0 MPa
@Strain 100 %
ISO 527-2/1A
 45.0 MPa
@Strain 10 %
ISO 527-2/1A
Elongation at Break 350 %50 mm / min. Nominal.; ISO 527-2/1A
Elongation at Yield 15 %ISO 527-2/1A
Tensile Modulus 1350 MPa1mm / min.; ISO 527-2/1A
Flexural Strength 50.0 MPa2mm / min.; ISO 178
Flexural Modulus 1260 MPa2mm / min.; ISO 178
Charpy Impact, Notched 10.0 kJ/m²ISO 179/1e/A
Tear Strength 249 kN/mISO 34-1
Abrasion 39ISO 4649
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+13 ohm-cm500V; IEC 60093
Surface Resistance 1.00e+12 ohm500V; IEC 60093
 
Thermal PropertiesOriginal ValueComments
Melting Point 219 °C10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 115 °CISO 75/2Bf
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °CISO 75/2Af
Vicat Softening Point 210 °C
@Load 5.10 kg
50°C/h; ISO 306
 
Processing PropertiesOriginal ValueComments
Melt Temperature 240 - 250 °CInjection Molding
Mold Temperature 30.0 - 50.0 °C
 
Descriptive Properties
Injection Molding Injection SpeedMedium

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PRADI6978 / 293483

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.