MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Total 4520WZ Polypropylene, Impact Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: ATOFINA 4520WZ polypropylene is a nucleated impact copolymer. 4520WZ is characterized by improved stiffness, creep resistance, high impact resistance, excellent antistatic properties and is formulated to allow faster cycling through early demolding.

Application

ATOFINA 4520WZ has been developed specifically for the injection molding of baskets, pails, toys and furniture.

Information provided provided by Total Petrochemicals.

Total Petrochemicals includes former Fina and Atofina plastics product lines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.905 g/ccASTM D1505
Melt Flow 7.0 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 3800 psiASTM D638
Elongation at Yield 7.0 %ASTM D638
Flexural Modulus 200000 psiASTM D 790
Izod Impact, Notched 150 J/mASTM D256
 55.0 J/m
@Temperature -20.0 °C
ASTM D256
Charpy Impact Unnotched 1.60 J/cm²Notched/Unnotched not specified; ASTM DIN53453
 0.600 J/cm²
@Temperature -20.0 °C
Notched/Unnotched not specified; ASTM DIN53453
 
Thermal PropertiesOriginal ValueComments
Melting Point 160 - 165 °CATOFINA Method
Deflection Temperature at 0.46 MPa (66 psi) 92.0 °CASTM D648
Vicat Softening Point 152 °CASTM D1525

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Total EVA 1020 VN 3 Ethylene Vinyl Acetate Copolymer - Blown Film
Total PSC 1340 Crystal Polystyrene
Total PSC 1160/1160N Crystal Polystyrene
Total Lacqtene® 1025 FH 24 LDPE blown film
Total Lacqtene® 1008 FE 30 LDPE blown film

PFINAA069 / 38505

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.