MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Matexcel MoS-026 TS-1 Molecular Sieve
Categories: Other Engineering Material

Material Notes: TS-1 is a titanium-silicon molecular sieve, belonging to the Pentasil type heteroatom molecular sieve, orthorhombic system, with a three-dimensional channel structure represented by ZSM-5, consisting of a "Z"-shaped channel and an elliptical straight channel intersecting with it. composition. The four-coordinated Ti in the framework of titanium-silicon molecular sieve TS-1 is the active center of selective oxidation reaction. In addition to maintaining the topological structure of the original MFI molecular sieve, TS-1 has special properties due to the uniform distribution of titanium atoms in the framework. The skeleton Si-O-Ti bond, which makes it have both catalytic oxidation activity and shape-selective catalytic performance. Due to the absence of strongly acidic A13+ ions in the skeleton structure, TS-1 has strong hydrophobicity and has unique catalytic performance for the shape-selective oxidation of various organic compounds with H2O2 participation. This new generation of shape-selective oxidation catalytic materials It is regarded as a new catalyst in the field of green chemistry technology. TS-1 molecular sieves have been used in the epoxidation of olefins, the ammoxidation of cyclohexanone, the oxidation of alcohols, the oxidation of saturated hydrocarbons and the hydroxylation of aromatic hydrocarbons (phenol and benzene).

Morphology: Powder

Key Words: Synonyms: TS-1 Molecular Sieve
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Descriptive Properties
Product overviewAperture Aperture (nm): 0.56-0.58 Si-Ti ratio SiO2/TiO2: 30~100 BET specific surface area (m2/g): >350 Relative crystallinity (%): >95 Burn reduction (%): <5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMXCK2045 / 300676

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.