MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Wacker Geniosil® GF 62 Silane
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Empirical formula: C8H12O6Si

CAS No.: 4130-08-9

Properties: The use of GENIOSIL® GF 62 as a crosslinker in acetoxy-crosslinking silicone systems permits selective adjustment of the crosslinking density and – in conjunction with additional additives - control of the crosslinking speed. Use of GENIOSIL® GF 62 in mineral-filled polymers (e.g. polymer filled with kaolin, ATH or magnesium hydroxide) leads to a marked improvement in the mechanical and electrical properties, as well as to increased moisture resistance in particular. In addition, the particles are rendered strongly water repellent, which results in improved filler dispersibility, reduced melt viscosity and thus easier processing. Use of GENIOSIL® GF 62 as a comonomer in polymers produces binders which exhibit much greatly improved wet scrub resistance and higher scratch resistance, for example, thanks to crosslinking and strong adhesion to the substrate.

Special features: GENIOSIL® GF 62 is a vinylacetoxysilane. It´s a corrosive, clear, colorless to slightly yellow liquid with a characteristic vinegarlike odor. It hydrolyzes in the presence of moisture (acetic acid is released) to form silanols, which can react with themselves to produce siloxanes or bind to inorganic substrates. As a bifunctional, organically unsaturated molecule, GENIOSIL® GF 62 is able to function as a molecular bridge between inorganic and organic substrates.

Application: GENIOSIL® GF 62 is mainly used in acetoxycrosslinking silicone sealants, in which it functions as a crosslinker and/or adhesion promoter. In addition, GENIOSIL® GF 62 is used in the production of surface-modified fillers, as a water scavenger and as a primer component.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.16 g/ccDIN 51757
Molecular Weight 232.3 g/mol
 
Thermal PropertiesOriginal ValueComments
Melting Point 7.00 °C
Boiling Point 112 °C
@Pressure 0.00130 MPa
Flash Point 110 °CISO 3679
Ignition Temperature 400 °Cliquids; DIN 51794
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.42DIN 51423
 
Descriptive Properties
Content<100 mg/kgHydrolyzable chloride (as HCl)
Purity>90%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PWACK9313 / 204842

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.