MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Master Bond UV15-7NV One part high performance UV epoxy system
Categories: Polymer; Thermoset; Epoxy; Epoxy Encapsulant, Unreinforced

Material Notes: Key Features:
  • Low viscosity
  • Superior non-yellowing properties
  • Excellent physical properties, enhanced durability and toughness
  • Low shrinkage upon cure
Master Bond UV15-7NV is a one component, UV curable polymer system for high performance bonding, sealing, coating and encapsulation. Its most salient features include superior physical strength properties, low shrinkage upon curing and good non-yellowing stability. This system bonds well to a wide variety of similar and dissimilar substrates including glass, metals and plastics, such as polycarbonates, acrylics and a number of polyester films. It is 100% reactive and does not contain any solvents or diluents. UV15-7NV offers very good chemical resistance to water, fuels and many solvents. The UV cured polymeric material can be employed over the wide service temperature range of -80°F to +300°F. UV15-7NV exhibits an excellent combination of properties including outstanding toughness, electrical insulation and withstanding thermal cycling. Master Bond UV15-7NV system is not oxygen inhibited and cures readily in 10-30 seconds when exposed to a UV light source emitting at a wavelength of 320-365 nm with an energy output as low as 20-40 milliwatts/cm². The rate of cure depends upon the compound’s distance from the light source, the thickness of the section and of course the intensity of the light source. The system can cure in sections up to 1/8 inch. However, when bonding, sections of a few thousandths of an inch are more than adequate. This system is widely used in optical, fiberoptic, electronic, laser, microelectronic and semiconductor applications.

Product Advantages:

  • One component system; no mixing needed
  • Exceptionally fast cure upon exposure to a UV light source at ambient temperatures
  • No air inhibition while curing; no special inert atmosphere required
  • Very good electrical insulator
  • High bond strength; excellent adhesion to many substrates
  • Good dimensional stability
  • Outstanding clarity and light transmission

Information provided by Masterbond.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.125 g/cc
Viscosity 4000 - 9000 cP
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 70 - 80
Tensile Strength 6000 - 7000 psi
Tensile Modulus 300000 - 350000 psi
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+14 ohm-cm
Dielectric Constant 3.5
@Frequency 60 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 55.0 - 60.0 µm/m-°C
Maximum Service Temperature, Air 300 °F
Minimum Service Temperature, Air -80.0 °F
Glass Transition Temp, Tg 65.0 - 70.0 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.54
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 MonthIn original unopened containers
 
Descriptive Properties
Colortransparentcured

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMASTM729 / 233786

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.