MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Electrolytic Tough Pitch (ETP) Copper, UNS C11000, H80 (16%) Temper flat rod
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Good to excellent corrosion resistance. Excellent hot and cold workability; good forgeability. Fabricated by coining, coppersmithing, drawing and upsetting, hot forging and pressing, spinning, swaging, stamping.

Applications: downspouts, gutters, roofing, gaskets, auto radiators, busbars, nails, printing rolls, rivets, and radio parts.

Test specimens: rod - 50mm diameter

Key Words: ASTM-B-152, QQ-C-576, CDA 110 ETP, C101, ISO Cu-ETP
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 8.89 g/cc
 7.93 g/cc
@Temperature 1083 °C
Liquid
 8.32 g/cc
@Temperature 1083 °C
Solid
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 45
Hardness, Rockwell F 85
Tensile Strength, Ultimate 310 MPa
 235 MPa
@Temperature -40.0 °C
 260 MPa
@Temperature -75.0 °C
 285 MPa
@Temperature -120 °C
 320 MPa
@Temperature 12.0 °C
 325 MPa
@Temperature -12.0 °C
 400 MPa
@Temperature -175 °C
Tensile Strength, Yield 275 MPa
@Strain 0.5 %
 65.0 MPa
@Strain 0.1 %,
Temperature 0.000 °C
 70.0 MPa
@Strain 0.1 %,
Temperature -50.0 °C
 75.0 MPa
@Strain 0.1 %,
Temperature -100 °C
 80.0 MPa
@Strain 0.1 %,
Temperature -150 °C
Elongation at Break 20 %In 50 mm
 40 %
@Temperature -12.0 °C
 45 %
@Temperature -120 °C
 47 %
@Temperature 12.0 °C
 48 %
@Temperature -40.0 °C
 48 %
@Temperature -75.0 °C
 57 %
@Temperature -175 °C
Reduction of Area 70 %
@Temperature -120 °C
 74 %
@Temperature -75.0 °C
 76 %
@Temperature 12.0 °C
 77 %
@Temperature -175 °C
 77 %
@Temperature -40.0 °C
 78 %
@Temperature -12.0 °C
Modulus of Elasticity 115 - 130 GPa
Poissons Ratio 0.33
Fatigue Strength 93.0 MPa
@Temperature 100 °C,
# of Cycles 1.00e+7 ,
Diameter 2.00 mm
Rotating-beam H80 wire
 95.0 MPa
@Temperature 65.0 °C,
# of Cycles 1.50e+7 ,
Diameter 2.00 mm
Rotating-beam H80 wire
 103 MPa
@Temperature 100 °C,
# of Cycles 7.50e+6 ,
Diameter 2.00 mm
Rotating-beam H80 wire
 105 MPa
@Temperature 65.0 °C,
# of Cycles 1.25e+7 ,
Diameter 2.00 mm
Rotating-beam H80 wire
 105 MPa
@Temperature 21.0 °C,
# of Cycles 1.00e+8 ,
Diameter 2.00 mm
Rotating-beam H80 wire
 110 MPa
@Temperature 100 °C,
# of Cycles 5.00e+6 ,
Diameter 2.00 mm
Rotating-beam H80 wire
 115 MPa
@Temperature 21.0 °C,
# of Cycles 5.00e+7 ,
Diameter 2.00 mm
Rotating-beam H80 wire
 115 MPa
@Temperature 65.0 °C,
# of Cycles 1.00e+7 ,
Diameter 2.00 mm
Rotating-beam H80 wire
 125 MPa
@Temperature 65.0 °C,
# of Cycles 7.50e+6 ,
Diameter 2.00 mm
Rotating-beam H80 wire
 130 MPa
@Temperature 21.0 °C,
# of Cycles 1.00e+7 ,
Diameter 2.00 mm
Rotating-beam H80 wire
 150 MPa
@Temperature 21.0 °C,
# of Cycles 5.00e+6 ,
Diameter 2.00 mm
Rotating-beam H80 wire
 167 MPa
@Temperature 21.0 °C,
# of Cycles 2.50e+6 ,
Diameter 2.00 mm
Rotating-beam H80 wire
Machinability 20 %UNS C36000 (free-cutting brass) = 100%
Forgeability 65 %UNS C37700 (forging brass) = 100%
Shear Modulus 44.0 - 49.0 GPadepending on temper
Shear Strength 180 MPa
Coefficient of Friction, Dynamic 0.29Sliding, with cast iron, no lubrication
 0.36Sliding, with carbon steel, no lubrication
 0.53Sliding, with glass, no lubrication
Coefficient of Friction, Static 0.53With carbon steel, no lubrication
 0.68With carbon steel, no lubrication
 1.05With cast iron, no lubrication
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000170 ohm-cm101% IACS
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 205 J/g
CTE, linear 17.0 µm/m-°C
@Temperature 20.0 - 100 °C
 17.3 µm/m-°C
@Temperature 20.0 - 200 °C
 17.7 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.385 J/g-°C
Thermal Conductivity 300 W/m-K
@Temperature 700 °C
 300 W/m-K
@Temperature -268.8 °C
 370 W/m-K
@Temperature 300 °C
 380 W/m-K
@Temperature 100 °C
 388 W/m-K
@Temperature 20.0 °C
 390 W/m-K
@Temperature 0.000 °C
 400 W/m-K
@Temperature -79.0 °C
 550 W/m-K
@Temperature -196 °C
 1300 W/m-K
@Temperature -253 °C
Melting Point 1065 - 1083 °C
Solidus 1065 °CEutectic
Liquidus 1083 °C
Softening Point 360 °C
Annealing Point >= 700 °F
 
Processing PropertiesOriginal ValueComments
Annealing Temperature 475 - 750 °C
Hot-Working Temperature 750 - 875 °C
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu >= 99.90 %includes Ag
Oxygen, O 0.040 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Electrolytic Tough Pitch (ETP) Copper, UNS C11000, H80 (35%) Temper flat rod
Electrolytic Tough Pitch (ETP) Copper, UNS C11000, H80 (40%) Temper flat rod, tube
Electrolytic Tough Pitch (ETP) Copper, UNS C11000, OSO50 Temper flat products, rod, tube, shapes
Electrolytic Tough Pitch (ETP) Copper, UNS C11000, H02 Temper flat products
Electrolytic Tough Pitch (ETP) Copper, UNS C11000, M20 Temper flat products, rod, shapes

MC11000c9 / 10505

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.