System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Copper, UNS C65400, H06 Temper strip
Categories:
Metal
;
Nonferrous Metal
;
Copper Alloy
Material Notes:
Good to excellent corrosion resistance. Excellent hot and cold workability.
Applications:
contact springs, connectors, and wiring devices
Test specimen: strip.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
8.55
g/cc
Mechanical Properties
Original Value
Comments
Hardness, Rockwell B
99
Tensile Strength, Ultimate
825
MPa
Tensile Strength, Yield
760
MPa
Elongation at Break
5.0 %
In 50 mm
Modulus of Elasticity
117
GPa
Machinability
30 %
UNS C36000 (free-cutting brass) = 100%
Electrical Properties
Original Value
Comments
Electrical Resistivity
0.0000246
ohm-cm
@Temperature 20.0 °C
Thermal Properties
Original Value
Comments
CTE, linear
17.5
µm/m-°C
@Temperature 20.0 - 300 °C
Thermal Conductivity
36.0
W/m-K
Melting Point
955
-
1020
°C
Solidus
955
°C
Liquidus
1020
°C
Annealing Point
750
-
1100
°F
Processing Properties
Original Value
Comments
Annealing Temperature
400
-
600
°C
Component Elements Properties
Original Value
Comments
Chromium, Cr
0.10 %
Copper, Cu
95.4 %
Silicon, Si
3.0 %
Tin, Sn
1.5 %
References
for this datasheet.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
MC65400b5 / 11647
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.