Applications:- Displays
- Personal care and Cosmetics
Product Description: Eastar Copolyester DN004HF has excellent flow characteristics while maintaining superior mechanical properties. It is easy to process and can fill intricate tools. Its most outstanding features are clarity, toughness and chemical resistance. DN004HF contains a mold release. This product has been GREENGUARD INDOOR AIR QUALITY CERTIFIED®. Information provided by Eastman. |