MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Silicon Carbide, SiC (Moissanite)
Categories: Ceramic; Carbide

Material Notes: Natural moissanite occurs as hard green-black hexagonal crystals. Colorless synthetic crystals are used as gemstones.

Key Words: Silicon Carbide
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.16 g/cc
Molecular Weight 40.097 g/mol
 
Mechanical PropertiesOriginal ValueComments
Hardness, Mohs 9.5
 
Electrical PropertiesOriginal ValueComments
Magnetic Susceptibility -0.0000128cm^3/mol
 
Thermal PropertiesOriginal ValueComments
Melting Point 2830 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 2.691ω, Na
 2.648
@Wavelength 589.3 nm
η, Na
 
Descriptive Properties
CAS Number409-21-2
ColorGreen blackCommon for natural specimens
Crystal StructureHexagonal

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Silicon Carbide, CVD
Silicon Carbide, Alpha SiC
Silicon Carbide, sublimed
Tungsten Carbide, WC
Chromium (III) Oxide, Cr2O3 (Eskolaite)

EINOR0720 / 3852

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.