System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Covestro Bayblend® KU2-1500 Polycarbonate + ABS Blend, Extrusion/Blow-Molding
(discontinued **)
Categories:
Polymer
;
Thermoplastic
;
ABS Polymer
;
Polycarbonate/ABS Alloy, Unreinforced
;
Polycarbonate (PC)
Material Notes:
Information provided by Bayer Corporation, Plastics Division
As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This product was discontinued prior to the separation.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.21
g/cc
ASTM D792
Spiral Flow
25.0
cm
@Thickness 2.50 mm
at 254°C melt temp.
Mechanical Properties
Original Value
Comments
Tensile Strength, Ultimate
52.0
MPa
ASTM D638
Tensile Strength, Yield
53.0
MPa
ASTM D638
Elongation at Break
90 %
ASTM D638
Elongation at Yield
3.8 %
ASTM D638
Flexural Yield Strength
87.0
MPa
at 5% strain; ASTM D790
Flexural Modulus
2.27
GPa
ASTM D790
Izod Impact, Notched
6.90
J/cm
@Thickness 3.17 mm
ASTM D256
Impact Test
52.0
J
@Thickness 3.20 mm
Instrumented Total Impact; 3.2 mm thick, 12.5 mm dart, 75 mm clamp, 6.7 m/s; ASTM D3763
Electrical Properties
Original Value
Comments
Arc Resistance
<=
60
sec
@Thickness 3.00 mm
UL Rating PLC 7 (<60 sec)
Comparative Tracking Index
>=
600
V
@Thickness 3.00 mm
UL Rating PLC 0 (>600 V)
Hot Wire Ignition, HWI
60
-
120
sec
@Thickness 3.00 mm
UL Rating PLC 1 (60-120 sec)
High Amp Arc Ignition, HAI
>=
120
arcs
@Thickness 1.50 mm
UL Rating PLC 0 (>120 arcs)
High Voltage Arc-Tracking Rate, HVTR
>=
150
mm/min
@Thickness 3.00 mm
UL Rating PLC 4 (>150 mm/min.)
Thermal Properties
Original Value
Comments
Deflection Temperature at 1.8 MPa (264 psi)
105
°C
@Thickness 6.35 mm
Unannealed; ASTM D648
Vicat Softening Point
129
°C
Rate B; ISO 306
UL RTI, Electrical
85.0
°C
@Thickness 1.57 mm
Bayer provisional value
UL RTI, Mechanical with Impact
75.0
°C
@Thickness 1.57 mm
Bayer provisional value
UL RTI, Mechanical without Impact
85.0
°C
@Thickness 1.57 mm
Bayer provisional value
Flammability, UL94
V-0
@Thickness 1.50 mm
V-0
@Thickness 1.50 mm
**
Materials flagged as discontinued (
) are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.
Users of our Advanced Search (registration required) may exclude discontinued materials from search results.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Covestro Makrolon® 3207 Polycarbonate
Covestro Makrolon® 2608 Polycarbonate
Covestro Makrolon® 1952 Polycarbonate
Covestro Makrolon® 1837 MAS081 Polycarbonate
Covestro Makrolon® 1239 Polycarbonate, Blow Molding/Extrusion Grade
PB1B09 / 26402
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.