MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Parker Chomerics CHO-SHIELD® 4966 Conductive Silicone Coating  (discontinued **)
Categories: Polymer; Adhesive; Thermoset; Silicone

Material Notes: Conductive Silicone Coating. This is a conductive silver-filled silicone coating. This three-component system is capable of providing 60 dB of shielding effectiveness above 30 MHz. The coating utilizes heat for cure which will vary with substrates. CHO-SHIELD 4966 is designed for coating silicone based substrates.

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 3.22 - 3.42 g/cc
Solids Content 72 %
Volatile Organic Compounds (VOC) Content 83 g/l
Brookfield Viscosity 100 cP@ 100 rpm, #2
Thickness 2.00 mil
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square <= 0.15 ohm
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 100 °C
Minimum Service Temperature, Air -40.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 30.0 min
Pot Life 300 min
Working Life 300 min
Shelf Life 6.00 Month
 
Descriptive Properties
BinderSilicone
ConsistencyThin Fluid
FillerAg
Mix Ratio100:15.1:2.6
ResinSilicone Polymer
Spraying Viscosity, #2 Zahn Cup, sec18 - 20
Theoretical Coverage ft^2/gal75

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCHOME167 / 28389

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.