MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Mo-Sci Corporation GL 1661 Hyroxyapatite Bioactive Glass
Categories: Ceramic; Glass

Material Notes: A porous object composed of nanosize hydroxyapatite crystals with white color in powder or spherical form. Applications: Healthcare; an absorber for ions, molecules, and drugs; environmental remediation; etc. Bioactive glasses have the ability to bond to soft and/or hard tissue and are biodegradable in the body. The release of ions and the formation of hydroxyapatite support the regeneration of bone tissue and can accelerate the healing process. These glasses are made from high purity (analytical and reagent grade) chemicals, keeping unwanted trace impurities to a minimum. Precious metal or high purity ceramic crucibles are used to melt these glasses in dedicated furnaces and they are processed in an environmentally controlled space.

Information provided by Mo-Sci Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density <= 0.900 g/cc
Specific Surface Area >= 120 m²/g
 
Component Elements PropertiesOriginal ValueComments
CaO 55.82 %
H2O, Water 1.79 %
P2O5 42.39 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

CMOSCI9001 / 200216

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.