MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Plastcom SLOVALEN PH 78 FRT 5 Polypropylene Homopolymer, Halogen Free and Phosphor Free Flame Retardant  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Flame Retardant

Material Notes: Features

Modified homopolymer PP for injection moulding, contains the modifier of mechanical properties and non halogen and free phosphor flame retardant. Increased strength in comparison with unfilled PP. Applied in all industry branches. Increased strength, toughness, modulus in tension due to the modification. Delivered in natural and in the full RAL color scale.

Application: Injection Moulding

Information Provided by Plastcom spol. s r.o.

Key Words: PP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.18 g/ccSTN 64 0111
Linear Mold Shrinkage 0.0168 cm/cmSTN 64 0808
Linear Mold Shrinkage, Transverse 0.0175 cm/cmSTN 64 0808
Melt Flow 15 - 25 g/10 min
@Load 2.16 kg,
Temperature 230 °C
STN EN ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 20.0 MPaSTN EN ISO 527-2
Elongation at Break 3.0 %STN EN ISO 527-2
Tensile Modulus 1500 MPaSTN EN ISO 527-2
Flexural Strength 300 MPaSTN EN ISO 178
Flexural Modulus 1500 MPaSTN EN ISO 178
Charpy Impact Unnotched 10.0 kJ/m²
@Temperature -20.0 °C
STN EN ISO 179
 16.0 kJ/m²
@Temperature 23.0 °C
STN EN ISO 179
Charpy Impact, Notched 1.00 kJ/m²
@Temperature -20.0 °C
STN EN ISO 179
 2.00 kJ/m²
@Temperature 23.0 °C
STN EN ISO 179
 
Thermal PropertiesOriginal ValueComments
Melting Point 145 °CDSC; STN EN ISO 3146
Vicat Softening Point 150 °CB; STN EN ISO 306
Flammability, UL94 V-0
@Thickness 1.60 mm
Glow Wire Test 960 °C3mm; STN IEC 60695-2-10
 
Processing PropertiesOriginal ValueComments
Melt Temperature 200 - 250 °C
Mold Temperature 40.0 - 80.0 °C
Drying Temperature 80.0 °C
Dry Time 4 hour
Moisture Content 0.20 %STN EN ISO 960
Injection Pressure 70.0 - 120 MPa

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Plastcom SLOVALEN PH 76 FRD 3 PP, flame retardant
Multibase Multi-Flam™ 0302 PP NH Polypropylene
Multibase Multi-Flam™ 0220 PP Polypropylene
Multibase Multi-Flam™ 0206 PP Polypropylene
Multibase Multi-Flam™ 0501 PP Polypropylene

PPLACO097 / 106975

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.