Sequel 1718-UV YBTA thermoplastic polyolefin is typically used for automotive exterior applications that require dimensional stability over a broad temperature range. This material exhibits excellent processability and low-temperature properties. Applications: Automotive Parts, Exterior Automotive ApplicationsInformation provided by LyondellBasell. |