Moplen EP542R is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP542R is a block copolymer selected by customers for use in injection molding of washing machine tub, thin-walled packaging, parts of electrical appliances, housewares etc. Moplen EP542R resin meets the FDA requirements in the Code of Federal Regulations in 21 CFR 177.1520 for food contact. Product Features: Optimized balance of stiffness and toughness/Low warpage and fast cycle time/Good toughness/Good processability Typical Applications: Washing machine tub/Parts of electrical appliance/Housewares Information provided by PolyMirae |