MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Inno-Comp INNOPOL® CS 2-2130 30% Talc Filled Polypropylene Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 30% Talc Filler

Material Notes: INNOPOL® CS 2-2130 is a 30 % talc-filled polypropylene compound /PP-B TD30 (ISO 1043)/. This grade is available in natural and custom colored form.

INNOPOL® CS 2-2130 is recommended for producing injection molded automotive products where the required property is high stiffness besides low shrinkage and low temperature resistance.

Information provided by INNO-COMP

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.13 g/ccISO 1183
Melt Flow 20 g/10 min
@Load 2.16 kg,
Temperature 230 °C
nozzle diam 2.095 mm; ISO 1133
Storage Temperature <= 60.0 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Stress 28.0 MPa50 mm/min; ISO 527-1,-2
Elongation at Yield 3.0 %50 mm/min; ISO 527-1,-2
Tensile Modulus 3100 MPa1 mm/min; ISO 527-1,-2
Flexural Modulus 3200 MPaISO 178
Charpy Impact, Notched 2.00 kJ/m²
@Temperature -20.0 °C
ISO 179/1eA
 3.50 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 126 °CISO 75-1,-2
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 210 - 240 °CInjection
Middle Barrel Temperature 210 - 240 °CInjection
Front Barrel Temperature 210 - 240 °CInjection
Melt Temperature 230 - 250 °CInjection
Mold Temperature 15.0 - 50.0 °C
Moisture Content <= 0.070 %
 
Descriptive Properties
Resin DesignationPP-B TD30ISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Tisan TISOPLEN® 10% Talc Filled Heat Stabilized Copolymer Polypropylene
Inno-Comp INNOPOL® CS 2-3130 NU UV-Stabilized 30% Talc-Filled Polypropylene Block-Copolymer
Inno-Comp INNOPOL® CS 1-3130 30% Talc-Filled Polypropylene Homopolymer

PINNO906 / 150106

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.