Temper: Nominal Grain Size 0.025 mm Fabrication Properties: Excellent Suitability – Soldering, Brazing, Butt Weld, Capacity for Being Cold Worked; Good Suitability – Capacity for Being Hot Formed; Fair Suitability – Gas Shielded Arc Welding Common Fabrication Processes: Drawing; Etching; Forming and Bending; Heading and Upsetting; Hot forging; Piercing and Punching Typical uses: Clips; Contacts; Flat Cable; Springs; Trolley Wire; Resistance Welding Electrodes Applicable Specifications: Wire – Trolly ASTM B9, ASTM B105 |