MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
SABIC ULTEM™ Resin 9085 Polyetherimide (PEI) (Americas)
Categories: Polymer; Thermoplastic; Polyetherimide (PEI)

Material Notes: High flow Polyetherimide blend. Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke and flame evolution.

Features: High Stiffness,Hydrolytic Stability,Chemical Resistance,Low Smoke and Toxicity,Good Mechanicals in Broad Temperature Range,Low Creep Sensitivity,Low Shrinkage,Good metal adhesion,Amorphous,High Strength,High Heat Resistance,Good dimensional stability,Flame Retardant

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.34 g/ccASTM D792
Density 1.34 g/ccISO 1183
Moisture Absorption 0.0200 %Injection Molding
 0.0200 %Profile Extrusion
 0.170 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.39 %ISO 62-1
Viscosity 40 cP
@Load 5.00 kg,
Temperature 340 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 8.9 g/10 min
@Load 6.60 kg,
Temperature 295 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 71.0 MPa5 mm/min; ISO 527
 74.0 MPa5 mm/min; ASTM D638
Tensile Strength, Yield 84.0 MPa5 mm/min; ASTM D638
 88.0 MPa5 mm/min; ISO 527
Elongation at Break 50 %5 mm/min; ISO 527
 72 %5 mm/min; ASTM D638
Elongation at Yield 6.7 %5 mm/min; ISO 527
 7.0 %5 mm/min; ASTM D638
Tensile Modulus 3050 MPa1 mm/min; ISO 527
 3440 MPa5 mm/min; ASTM D638
Flexural Strength 90.0 MPayield, 2 mm/min; ISO 178
 138 MPayld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2750 MPa2 mm/min; ISO 178
 2920 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 115 JASTM D256
Izod Impact, Notched (ISO) 13.0 kJ/m²80*10*4; ISO 180/1A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 56.0 µm/m-°C
@Temperature -30.0 - 80.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 60.0 µm/m-°C
@Temperature -30.0 - 80.0 °C
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 152 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 153 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 173 °CRate B/120; ISO 306
Oxygen Index 49 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Processing Temperature 80.0 - 120 °CCalibrator 2 Temperature
 130 - 160 °CCalibrator Temperature
Nozzle Temperature 330 - 350 °C
Zone 1 265 - 275 °CProfile Extrusion
Zone 2 280 - 295 °CProfile Extrusion
 325 - 345 °C
Zone 3 290 - 305 °CProfile Extrusion
 330 - 350 °C
Zone 4 295 - 310 °CProfile Extrusion
Adapter Temperature 270 - 310 °CProfile Extrusion
Die Temperature 260 - 310 °CProfile Extrusion
Melt Temperature 280 - 310 °CProfile Extrusion
 330 - 350 °CInjection Molding
Mold Temperature 120 - 150 °C
Drying Temperature 120 - 130 °CProfile Extrusion
 135 °CInjection Molding
Dry Time 4.00 - 6.00 hourInjection Molding
 4.00 - 6.00 hourProfile Extrusion
Back Pressure 0.300 - 0.700 MPa
Shot Size 40 - 60 %
Vent Depth 0.00250 - 0.00760 cm
Screw Speed 40 - 70 rpm
Precipitation Temperature 80.0 - 100 °CHopper Temperature
 
Descriptive Properties
FAA Flammability, FAR 25.853 A/B<5FAR 25.853
OSU peak heat release rate (5 minute test)36 kW/m²FAR 25.853
OSU total heat release (2 minute test)16 kW-min/m²FAR 25.853
Vertical Burn a (60s) passes at2 SecondsFAR 25.853

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82561 / 290508

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.