MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ascend Performance Materials Vydyne® PIQ621 Nylon 66 Compounding Grade  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: Vydyne PIQ621 is a medium viscosity neat PA66 resin. It is available in natural and designed for applications ranging from cast film extrusion to extrusion compounding. This resin offers a well balanced combination of properties such as high strength, rigidity, good toughness/ductility, high melt point, good surface lubricity, and abrasion resistance. Vydyne PIQ621 maintains the chemical resistance typical of PA66 to many chemicals, machine and motor oils, solvents, and gasoline.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.674 g/ccASTM D1895
Density 1.14 g/ccISO 1183
Moisture Absorption <= 0.500 %ASTM D6869
Viscosity Measurement 48 - 52Relative Viscosity - Formic acid; ASTM D789
Viscosity Test 143 - 150 cm³/gViscosity Number (H2SO4, sulfuric acid); ISO 307
 
Thermal PropertiesOriginal ValueComments
Melting Point 260 °CISO 11357-3
 
Optical PropertiesOriginal ValueComments
Yellow Index <= -4.00 %ASTM D1925
 
Compliance PropertiesOriginal ValueComments
FDA Yes21 CFR 177.1500
 
Descriptive Properties
Agency RatingsEU 10/2011
 EU 2023/2006
FeaturesGeneral Purpose
 Good Abrasion Resistance
 Good Chemical Resistance
 Good Toughness
 High Rigidity
 High Strength
 Low Viscosity
 Oil Resistant
 Solvent Resistant
UsesCast film
 Compounding
 General Purpose

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PZASCE9917 / 220967

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.