Available as Flame Retardant Catalyst Masterbatch component for PolyOne Syncure System. Gel, Torque, Dispersion, and Oven Aging were measured on a 100 phr S1027A / 66.7 phr V0064G Syncure System. Cured for 8 hours in steam at 90°C for Gel test and Oven Aging. Torque is > 900. Dispersion is Visual. Pellet appearance is 1/8 round. Information provided by PolyOne |