Hostacom TRC 104N is a 20% talc filled elastomeric modified PP, with excellent processability and excellent impact/stiffness balance. This grade is delivered in customer customized colors, some properties may be slightly altered upon color selected. Applications: Automotive Parts, Instrument Panels, Interior TrimsInformation provided by LyondellBasell. |