System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Ganpati Exim N339 Carbon Black
Categories:
Other Engineering Material
;
Additive/Filler for Polymer
Material Notes:
Fine reinforcing carbon black with increased structure. Provides high modulus, improved extrusion, wear resistance and hysteresis. Tire tread, retread compounds, industrial rubber goods, conveyor belts.
Information provided by Ganpati Exim PVT. LTD.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
0.315
-
0.375
g/cc
Pour
pH
6.0 - 8.0
Specific Surface Area
88
m²/g
External; Statistical Thickness Surface Area,; ASTM D 6556
88
-
98
m²/g
External
Ash
<= 0.45 %
Mechanical Properties
Original Value
Comments
300% Modulus
-2.70
-
-0.700
MPa
IRB 6
Descriptive Properties
Content
<1.1%
Sulphur
DBP Absorption Number
115-125 cm3/100g
DBP Absorption Number of Compressed Sample
99 cm3/100g
Fines Content
<6%
Pelleted
Heating Loss
<0.9%
Individual Pellet Hardness
25-100 g
Iodine Number
85-95 g/kg
Nitrogen Adsorption Number
91 m2/g
(D6556)
Sieve Residue
<0.001%
05
<0.1%
0045
Tint Index
1.11
ITRB
Toluene Discoloration
>87%
transmittance
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
PGANPATI005 / 317289
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.