MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Master Bond MB250NT Single Component Ethyl Cyanoacrylate
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: Key Features:
  • One component, no mix system
  • Non-toxic as per ISO 10993-5
  • Fast setting
  • Rapid fixture time
Product Description: Master Bond MB250NT is a single component ethyl cyanoacrylate type system. This rapid curing, high strength system is used primarily in applications where the ISO 10993-5 for low toxicity is specified. MB250NT has a low viscosity of 100-110 cps. Cyanoacrylates are commonly referred to as super glues or instant adhesives. Their curing is dependent upon the humidity with the higher the level, the faster the rate of cure. Since the cure is typically fast, only minimal contact pressure is required for bonding. There is no mixing or heating required for curing. Depending upon the humidity and the substrates, MB250NT will typically set up within 10-40 seconds. MB250NT bonds well to a variety of substrates especially metals, composites, plastics and rubbers, especially in the shear mode. The service temperature range for this system is -60°F to +250°F. MB250NT can be used in a wide array of different applications ranging from repair to high speed production in which the ISO specification is required. It has first rate resistance to EtO and gamma sterilization processes. Although many of the applications for MB250NT involve disposable type medical devices, it also can be utilized with reusable ones depending upon the service conditions.

Product Advantages:

  • Rapid curing at room temperature; usually sets up within 40 seconds
  • No heating or mixing
  • Contact pressure usually sufficient for fixturing
  • Bonds well to a wide variety of substrates
  • Excellent resistance to EtO and gamma sterilization
  • Well suited for disposable and reusable medical devices
  • Passes ISO 10993-5

Information provided by Master Bond Inc.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.05 g/cc
Viscosity 100 - 110 cP
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 70
Tensile Strength 5000 psi
Elongation at Break 2.0 - 3.0 %
Tensile Modulus 200000 - 250000 psi
Adhesive Bond Strength 210 psiButyl-Butyl, Tensile lap; Substrate Failure
 300 psiSteel-Natural Rubber, Tensile lap; Substrate Failure
 350 psiSteel-Butyl, Tensile lap; Substrate Failure
 420 psiNatural Rubber-Natural Rubber, Tensile lap; Substrate Failure
 440 psiSBR-SBR, Tensile lap; Substrate Failure
 470 psiNeoprene-Steel, Tensile lap
 510 psiNitrile-Nitrile, Tensile lap; Substrate Failure
 510 psiNBR-NBR, Tensile lap; Substrate Failure
 520 psiNeoprene-Neoprene, Tensile lap; Substrate Failure
 570 psiPolystyrene-Polystyrene, Tensile lap; Substrate Failure
 850 psiDelrin-Delrin, Tensile lap
 910 psiNylon-Bakelite, Tensile lap
 910 psiNylon-Nylon, Tensile lap
 970 psiNBR-Aluminum, Tensile lap
 1070 psiChromium-Chromium, Tensile lap
 1080 psiAluminum-Aluminum, Tensile lap
 1200 psiPhenolic-Phenolic, Tensile lap
 1250 psiABS-ABS, Tensile lap
 1410 psiNylon-Copper, Tensile lap; Substrate Failure
 1590 psiAluminum-Stainless Steel, Tensile lap
 1640 psiSteel-Stainless Steel, Tensile lap
 2050 psiSteel-PVC (rigid), Tensile lap; Substrate Failure
 2100 psiPolyester-Polyester, Tensile lap
 2320 psiSteel-Aluminum, Tensile lap
 2340 psiCopper-Copper, Tensile lap
 2360 psiStainless-Stainless, Tensile lap
 2370 psiBrass-Brass, Tensile lap
 2380 psiSteel-Steel, Tensile lap
 2670 psiPVC(rigid)-PVC(rigid), Tensile lap; Substrate Failure
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cm
Dielectric Constant 3.6
@Frequency 1000 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 70.0 - 75.0 µm/m-°C
Maximum Service Temperature, Air 250 °F
Softening Point 290 - 300 °F
Minimum Service Temperature, Air -60.0 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 0.167 - 0.250 minset up time, substrate dependent
Shelf Life 6.00 Monthin original, unopened containers
 
Descriptive Properties
ColorColorless, transparent liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Röchling LAMIGAMID® 410 Cast Polyamide 6, Elastomer Modified, Low Temp, Dry
Henkel Loctite® 417 General Purpose Ethyl Cyanoacrylate Bonding Adhesive
Henkel Loctite® 416 General Purpose Ethyl Cyanoacrylate Bonding Adhesive
Henkel Loctite® 414 General Purpose Ethyl Cyanoacrylate Bonding Adhesive
Henkel Loctite® 412 General Purpose Ethyl Cyanoacrylate Bonding Adhesive

PMASTM919 / 185512

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.