MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC GELOY™ CR7520 ASA (Americas)
Categories: Polymer; Thermoplastic; ASA Polymer

Material Notes: ASA. Profile and Sheet. Excellent weatherability, good flow/aesthetics and high impact.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.06 g/ccASTM D792
Moisture Absorption at Equilibrium 0.55 %ASTM D570
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 7.0 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ASTM D1238
 13 g/10 min
@Load 5.00 kg,
Temperature 260 °C
ASTM D1238
 19.5 g/10 min
@Load 3.80 kg,
Temperature 280 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 86ASTM D785
Tensile Strength at Break 30.0 MPa50 mm/min; ISO 527
 34.0 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 39.0 MPa50 mm/min; ISO 527
 41.0 MPa50 mm/min; ASTM D638
Elongation at Break 40 %50 mm/min; ASTM D638
 44 %50 mm/min; ISO 527
Elongation at Yield 3.1 %50 mm/min; ISO 527
Tensile Modulus 1790 MPa50 mm/min; ASTM D638
 2000 MPa1mm/min; ISO 527
Flexural Yield Strength 58.0 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 1790 MPa1.3 mm/min, 50 mm span; ASTM D790
 2000 MPa2 mm/min; ISO 178
Izod Impact, Notched 320 J/mASTM D256
 58.0 J/m
@Temperature -30.0 °C
ASTM D256
Izod Impact, Notched (ISO) 19.0 kJ/m²80*10*4; ISO 180/1A
 5.00 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Charpy Impact, Notched 17.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 35.0 JASTM D3763
 20.0 J
@Temperature -30.0 °C
ASTM D3763
 
Electrical PropertiesOriginal ValueComments
Surface Resistance >= 1.00e+15 ohmASTM D257
Dielectric Constant 3.21
@Frequency 1e+6 Hz
ASTM D150
 5.2
@Frequency 50.0 - 60.0 Hz
ASTM D150
Dielectric Strength 15.9 kV/mm
@Thickness 3.20 mm
in oil; ASTM D149
Dissipation Factor 0.026
@Frequency 1e+6 Hz
ASTM D150
 0.15
@Frequency 50.0 - 60.0 Hz
ASTM D150
Comparative Tracking Index >= 600 VUL 746A
Hot Wire Ignition, HWI 15 - 30 secUL 746A
High Amp Arc Ignition, HAI >= 120 arcsUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 84.6 µm/m-°C
@Temperature -30.0 - 0.000 °C
ASTM E831
 86.4 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 90.0 µm/m-°C
@Temperature 0.000 - 100 °C
ASTM E831
CTE, linear, Transverse to Flow 91.8 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 91.0 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 87.0 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 90.0 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 95.0 °Cannealed; ASTM D648
 76.0 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 79.0 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Vicat Softening Point 90.0 °CRate B/50; ISO 306
 99.0 °CRate B/50; ASTM D1525
UL RTI, Electrical 50.0 °CUL 746B
UL RTI, Mechanical with Impact 50.0 °CUL 746B
UL RTI, Mechanical without Impact 50.0 °CUL 746B
Flammability, UL94 HB
@Thickness 1.47 mm
UL 94
 
Optical PropertiesOriginal ValueComments
Gloss 95 %60°; ASTM D523
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 240 - 270 °CInjection Molding
Zone 1 220 - 250 °C
Zone 2 225 - 260 °C
Zone 3 240 - 270 °C
Melt Temperature 240 - 270 °C
Mold Temperature 55.0 - 75.0 °C
Drying Temperature 80.0 - 90.0 °CInjection Molding
Dry Time 3.00 - 6.00 hourInjection Molding
 12.0 hourCumulative; Injection Molding
Moisture Content 0.040 %
Back Pressure 0.700 - 1.40 MPa
Shot Size 40 - 80 %
Vent Depth 0.00380 - 0.00760 cm
Screw Speed 30 - 80 rpm
 
Descriptive Properties
UV-light, water exposure/immersionF2UL 746C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10125 / 243592

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.