MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Go Yen Chemical GY-S-6042 Organicsilicon
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: GY-S-6042 silane offers consistent and dramatic improvements in water stable adhesion performance.

Applications: Silane coupling agent GY-S-6042, is an excellent candidate for formulations employing carboxylated latexes (acrylic, SBR polyurethane, etc. ) exhibiting a pH between 6 and 8.5. GY-S-6042 silane can be employed as an adhesion promoter or crosslinker. It may be suitable for use as a water stable single component crosslinker in applications such as:

  • Automotive laminate adhesives.
  • Furniture laminate adhesives.
  • Flocking adhesives.
In such applications, GY-S-6042 silane should provide a means of replacing a 2 part waterborne adhesive with a single component system. The benefits of a silane crosslinked water stable single component system include reduced scrap, improved process efficiency and reduced crosslinker toxicity. As an adhesion promoter for waterborne systems such as the acrylic sealant, GY-S-6042 silane offers consistent and dramatic improvements in water stable adhesion performance.

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.979 g/cc
Viscosity 3.0 cP
Molecular Weight >= 248.39 g/mol
 
Thermal PropertiesOriginal ValueComments
Flash Point 140 °C
 
Descriptive Properties
Purity>95%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGOYEN693 / 267001

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.