MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC LNP™ THERMOCOMP™ Compound IF00C Polyamide 612 (Nylon 612)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 612 (PA612)

Material Notes: LNP THERMOCOMP IF00C is a compound based on Nylon 6/12 resin containing 60% Glass Fiber.

Features: High Stiffness,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.68 g/ccASTM D792
Density 1.67 g/ccASTM D792
Moisture Absorption 0.100 %23°C/50% RH/24 hrs; ASTM D570
 0.130 %23°C / 50% RH; ISO 62
 0.120 - 0.200 %Injection Molding
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.0060 - 0.0080 cm/cm24hrs; ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 202 MPa5 mm/min; ISO 527
 207 MPa5 mm/min; ASTM D638
Elongation at Break 1.9 %5 mm/min; ISO 527
 2.0 %5 mm/min; ASTM D638
Tensile Modulus 20070 MPa1 mm/min; ISO 527
 21440 MPa5 mm/min; ASTM D638
Flexural Strength 306 MPaISO 178
 311 MPabrk, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 18240 MPa2 mm/min; ISO 178
 18500 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 137 JASTM D256
Izod Impact, Unnotched 1050 J/mASTM D4812
Izod Impact, Notched (ISO) 13.0 kJ/m²80*10*4; ISO 180/1A
Dart Drop, Total Energy 10.0 JASTM D3763
Impact Test 3.00 JMultiaxial Impact; ISO 6603
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 22.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
ASTM D696
CTE, linear, Transverse to Flow 53.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 214 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 215 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 198 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 205 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Zone 2 260 - 270 °C
Zone 3 270 - 280 °C
Melt Temperature 270 - 275 °CInjection Molding
Mold Temperature 65.0 - 95.0 °C
Drying Temperature 80.0 °CInjection Molding
Dry Time 4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa
Screw Speed 30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH81620 / 289567

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.