MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ed Fagan Alloy 52 Controlled Expansion Alloy
Categories: Metal; Electronic/Magnetic Alloy; Ferrous Metal

Material Notes: Used in glass seals and a wide variety of other electronic applications. Similar to Pernifer 50 and NILO 50.

Information provided by Ed Fagan, Inc.

Key Words: ASTM F-30, MIL 1-23011 CL 2, AMS 1-23011 CL 2
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.300 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 80
Tensile Strength, Ultimate 552 MPa
Tensile Strength, Yield 276 MPa
Elongation at Break 35 %in 2"
Modulus of Elasticity 159 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000440 ohm-cm
Curie Temperature 530 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.0 µm/m-°C
@Temperature 30.0 - 500 °C
 10.1 µm/m-°C
@Temperature 30.0 - 400 °C
 10.1 µm/m-°C
@Temperature 30.0 - 475 °C
 10.2 µm/m-°C
@Temperature 30.0 - 300 °C
 10.2 µm/m-°C
@Temperature 30.0 - 350 °C
 10.4 µm/m-°C
@Temperature 30.0 - 200 °C
 10.4 µm/m-°C
@Temperature 30.0 - 250 °C
 10.4 µm/m-°C
@Temperature 30.0 - 525 °C
 10.5 µm/m-°C
@Temperature 30.0 - 100 °C
 10.5 µm/m-°C
@Temperature 30.0 - 150 °C
 10.8 µm/m-°C
@Temperature 30.0 - 600 °C
 11.7 µm/m-°C
@Temperature 30.0 - 700 °C
 12.5 µm/m-°C
@Temperature 30.0 - 800 °C
 13.3 µm/m-°C
@Temperature 30.0 - 900 °C
 14.2 µm/m-°C
@Temperature 30.0 - 1000 °C
Thermal Conductivity 97.0 BTU-in/hr-ft²-°F
Melting Point 1427 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.05 %
Iron, Fe 49.5 %as Balance
Nickel, Ni 51 %
Silicon, Si <= 0.30 %
Sulfur, S <= 0.025 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Carpenter Hiperco® Alloy 50 Fe-Co-V Soft Magnetic Alloy, Cold Rolled
Kanthal® 52 Nickel-Iron Resistor Alloy
Nickel Iron Alloy 52 Sealing Wire, UNS N14052
Aperam FeNi 70 Controlled Expansion Alloys Iron-Nickel Alloys
Aluminum 6061-T6; 6061-T651

NEDFA9952 / 194971

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.